← All linesProduct line
SoftSkin-contact & wearable parts
Soft line
Built for wearables — skin-friendly and soft. Super-soft filaments are normally hard to print; TOPFOX Soft is modified to print easier and better than conventional ones.
- Ultra-soft and skin-friendly — wearables first (braces, liners)
- Modified formula prints easier and better than conventional soft filament
- Print difficulty: easy (close to PLA)
Print speed>40 mm/s
Hardness75A / 70A / 65A
DifficultyEasy ≈ PLA

Which shore hardness?
Same line, same formula — only firmness differs. See each hardness in a real print, then pick by what you're printing.

Orthotics, braces, liners and other skin-contact, wearable products.
3 hardness options — same line, pick your firmness
75A70A65A
Diameter1.75 / 2.85 mm
Nozzle0.6 / 0.8 mm
Four common pitfalls, solved
Know the cause before it happens.
Moisture
SYMPTOMIncreased stringing, bubbles/rough surface, nozzle hissing
CAUSETPU absorbs moisture quickly
FIXDry at 70–75 °C for 4 h before printing; seal + desiccant; re-dry after 1–2 days exposed
Stringing
SYMPTOMThin wisps left on travel moves
CAUSEHigh temp / low retraction / moisture / Z-hop
FIXDry first → drop 5 °C → enable Combing → disable Z-hop → add slight retraction; clean with a heat gun
Soft-filament feeding
SYMPTOMExtruder gear clicking, filament wrapping the gear
CAUSEToo much retraction / gear too tight / sudden speed changes
FIXLess retraction (0.5–1.5 mm), loosen the gear, prefer direct drive, keep speed uniform
Layer adhesion
SYMPTOMBreaks along layer lines when bent
CAUSELow temp / strong fan / too fast / moisture
FIXRaise 5–10 °C, fan <30%, slow down, dry
Which line is right for you?
Three lines, three tuning directions — pick what matters most.
| Line | Speed | Hardness | Core goal | Action |
|---|---|---|---|---|
| Fast (Standard) | 140 mm/s | 95A / 90A / 85A / 80A | Reliable, with speed | View → |
| Ultra-Fast (High-Speed) | 240 mm/s | 95A / 90A / 85A | Maximize print speed | View → |
| Soft (Flexible)Current | >40 mm/s | 75A / 70A / 65A | Soft & skin-friendly | You're here |
| High-Elastic (Rebound) | 120 mm/s | 95A / 95A Pro / 95A Pro+ | High rebound, deformation-resistant | View → |
| AMS Edition | 140 mm/s | 95A / 68D | Bambu AMS compatibility | View → |
Speed data is based on TOPFOX lab tests. Actual results depend on the printer, model geometry and slicing parameters.
Specification
Diameter1.75 mm ± 0.03 mm
Net weight1 kg / 250 g (AMS: up to 3 kg)
Nozzle temp220–260 °C
Print difficultyEasy after drying (≈ PLA)
Storage15–30 °C, <30% RH, sealed + desiccant
Drying70–75 °C · 4 h
Spool size20.5 × 20.5 × 7 cm
Downloads
Files coming soon
Print settings PDFPreparing
Color card PDFPreparing
Slicer profilesPreparing
Test basis
Certified data and reports — to be published.
- Tensile strength
- TBD
- Elongation at break
- TBD
- Rebound rate
- TBD
- Batch consistency
- TBD
- Certifications (REACH / RoHS)
- TBD
FAQ
How to store TPU filament?
· 密封袋/密封盒 + 干燥剂(硅胶)
· 湿度 > 40% 的环境建议使用干燥箱打印
· 暴露空气中超过 1–2 天就需要重新干燥
· 远离阳光直射和高温
黄金法则:取出打印后立即放回密封袋并封好口。
What is the shelf life of TPU?
· 干燥密封状态:1–2 年没问题
· 暴露潮湿环境:几天就会吸湿到影响打印的程度
过期或严重受潮的 TPU 不一定报废——充分干燥(55°C / 6小时)后仍可使用。判断标准:打印时无嘶嘶声、表面无气泡。
Can I mix TPU from different brands?
物理上可以(都是 TPU 基材),但不同品牌的打印参数可能差异较大:
· 不建议在同一卷上拼接不同品牌的线材
· 切换品牌时建议重新做温度塔测试
· 同一打印任务中尽量使用同一品牌同一批次
Can TPU prints be post-processed?
· 打磨:不推荐——TPU 太软,砂纸会把表面拉毛
· 喷漆:用柔性漆(flexible paint)
· 粘接:TPU 专用胶或火焰处理 + 聚氨酯胶
· 去拉丝:热风枪/打火机快速过一遍(最有效方法)
· 涂层:聚氨酯清漆可以增加表面硬度和耐刮性
Is TPU resistant to oil and chemicals?
· 良好抗性:大多数油类、油脂
· 可耐受:弱酸弱碱、汗液、雨水、普通清洁剂
· 不耐受:强酸强碱、某些有机溶剂(如 THF、DMF)
日常使用中,TPU 对汗液和雨水的耐受性很好,非常适合穿戴类应用。
Feel it before you commit
Request a Soft line sample and experience the print quality yourself.